Ti-Nanoxide T600/SC is a solution for the formation of 600 nm thick mesoporous titania layers by spin-coating (5000 rpm for 30 s, acceleration 2000 rpm/s) and firing at 475°C for 30 min. The mesoscopic structure obtained by the sintering of nano-particles in the process makes a perfect host for perovskite crystals.
What's more, advanced users can advantageously tune the thickness of their mesoporous films by adjusting the concentration of Ti-Nanoxide T600/SC with the help of ethanol and the calibration curve shown below.
- Intended for :
- spin-coating
- Resulting layer :
- highly transparent
- Anatase particles :
- 15-20 nm
- Diffusing particles :
- none
- Concentration :
- 7% wt.
- Medium :
- alcohol, water, organic binders
- Treatment :
- high temperature required